Two-component spraying marking construction in Shunyi District, Beijing
 |
Construction time: May 9, 2019
Construction temperature: 15°C
Construction material: SW402
Spreading process: Glass beads are sprinkled on the pressurized surface
|
Construction Notes
Night construction, departure at half past six in the evening, and end at five in the morning.
Graco's original internal mixing gun was used, and the A and B components of the coating were well mixed and the curing time did not exceed ten minutes.
Lower ambient temperatures may slightly affect atomization, consider adding diluent.
The laser ruler plays an obvious role in the night construction process.
Live recording