Two-Component Sling-Coating Marking Project in Leshan, Sichuan
 |
Construction Date: December 29, 2017
Construction Temperature: 13℃
Construction Material: SP208
Sprinkling Process: Surface Sprinkling of Glass Beads |
Construction Notes
Construction was carried out during the daytime with relatively high temperatures, which significantly shortened the curing time. Attention should be paid to preventing curing-related risks.
The coating must be fully stirred before use, and the dosage of curing agent added to Component B must be fine-tuned based on real-time feedback.
Two-component sling-coating marking was adopted for the edge lines, which featured excellent line shape and outstanding drainage performance.
Thickness measurement and real-time quality inspection were conducted throughout the entire construction process.
On-site Records